Shrinkage characteristic of soft Bangkok clay stabilized by cement and fly ash

  • อนุพงศ์ คำปลอด สาขาวิศวกรรมโยธา คณะวิศวกรรมศาสตร์ มหาวิทยาลัยพะเยา
  • ธนกร ชมภูรัตน์
  • อภิชาต บัวกล้า
Keywords: soft Bangkok clay, cement, fly ash, image processing technology

Abstract

This article is to present the shrinkage characteristic of soft Bangkok clay stabilize with cement and fly ash by using image processing technique. The law materials consist of soft Bangkok clay, Portland cement type 1, and fly ash from Mae Moh Power Plant. The mix ratio of soft clay blended with cement is shown in term of the cement/clay-water ratio which are 0.3 and 0.4. From each mix ratio, fly ash is replaced in the amount of 0, 15, 30, 45, and 60%. For shrinkage analysis, the image processing method of 2D is used together with the PCAS and ImageJ software. The programs can analyze the number of cracks segment, crack length, crack width, and crack area as well as crack intensity factor. Finally, this study will suggest the optimum mix ratio of soft Bangkok clay admixed with cement and fly ash for applying soil improvement practices.

Downloads

Download data is not yet available.
Published
2020-07-09
How to Cite
[1]
คำปลอดอ., ชมภูรัตน์ธ. and บัวกล้าอ. 2020. Shrinkage characteristic of soft Bangkok clay stabilized by cement and fly ash. The 25th National Convention on Civil Engineering. 25, (Jul. 2020), GTE47.

Most read articles by the same author(s)

1 2 > >>